Industrial Coating Fisheyes: Causes and Prevention

EFC Painting • November 24, 2026

Fisheyes in industrial coatings form when wet paint pulls away from small areas instead of spreading into a continuous film. Remaining grease or an unsuitable surface can cause this loss of wetting, but a crater's appearance alone doesn't establish the cause.

For a facility owner, these defects can mean interrupted work and a finish that needs repair. Stopping before the next coat helps keep a localized problem from becoming a larger recoating job.

Start by separating fisheyes from similar defects, then trace what contacted the surface before application.

Key Takeaways

  • Fisheyes are localized depressions where wet coating pulls back; some expose the underlying coat or substrate.
  • Prevention depends on surface cleaning, suitable preparation, clean application equipment, and protection against recontamination.
  • Corrective action starts with finding the cause. Adding another coat without addressing that cause can repeat the defect.

What Fisheyes Look Like in Industrial Coatings

Recognizing the pullback pattern

A fisheye usually appears as a small, rounded depression surrounded by coating. The wet film retreats from the affected spot, sometimes leaving a visible center where coverage is thin or absent.

Individual defects may appear across an otherwise smooth finish. In other cases, several develop within one contaminated area. Their depth matters because a shallow depression and an opening through the protective film require different assessments.

On equipment, steelwork, or coated floors, inspect both the appearance and continuity of the film. A cosmetic-looking crater may leave insufficient coverage where protection matters.

Separating fisheyes from other defects

Crater-shaped defects don't all develop for the same reason. Pinholes are small openings, while solvent popping can also leave holes or craters during or after application. Blisters are raised areas rather than simple depressions.

The timing of the defect helps narrow the investigation. Note whether the coating pulled away while wet or whether openings appeared later.

Our guide to distinguishing coating craters from other defects covers these overlapping appearances. A reliable diagnosis considers the application record and surrounding film, not just a close-up photograph.

Why the Coating Pulls Away

Remaining grease interrupts wetting

A coating needs to wet the surface before it can form an even film. Low-surface-tension contamination can disturb that wetting and cause the liquid coating to retreat locally.

Remaining grease is one practical concern. A surface may look clean while still carrying a thin residue that interferes with coverage. Painting over that residue leaves the underlying problem in place.

Cleaning therefore has to remove contamination, rather than spread it across a larger area. The cleaning method also needs to suit the substrate and coating system.

An unsuitable surface needs attention before painting

An existing finish or substrate may be unsuitable for the proposed coating without additional preparation. Cleanliness, surface condition, and compatibility all affect whether the next layer spreads and bonds properly.

FRP wall panels illustrate why appearance alone isn't enough. Their coating preparation requires attention to the existing surface and remaining grease. Our guidance on painting FRP panels in commercial kitchens includes inspecting primer for pullback before applying the finish.

When defects appear immediately after priming, pause the work. Covering them removes useful evidence without resolving the cause.

Prepare and Clean the Substrate Before Application

Remove residue before mechanical preparation

Cleaning and mechanical preparation have different jobs. Cleaning removes unwanted material, while abrasion or blasting develops the surface condition required by the coating system.

Start with a cleaning method suitable for the substrate. Use clean application materials, and replace cloths before they redistribute collected residue. Where the cleaning procedure requires rinsing, complete that step rather than leaving cleaner behind.

Avoid treating extra sanding as a substitute for degreasing. Working contamination into a prepared surface can make removal harder. On an existing coating, also address loose or unsound material before the next application.

The work area matters, too. Keep nearby operations from depositing fresh contamination while the surface is being prepared.

Remove dust and protect the prepared surface

Abrasive blasting can leave spent abrasive, broken coating, and fine debris. Loose dust can interfere with contact between the primer and steel, although dust alone doesn't establish a fisheye diagnosis.

Remove preparation debris before coating. Then protect the surface against settling dust and unnecessary handling.

Our guidance on checking steel cleanliness before coating explains why a clean appearance doesn't establish that preparation meets project requirements.

Inspect close to application time. A surface that was acceptable earlier can become dirty again while other work continues nearby.

Keep Air, Materials, and Spray Equipment Clean

Maintain the air supply and application equipment

Compressed air used for spraying or blowing off a prepared surface must be clean. Otherwise, the cleanup or application process can reintroduce unwanted material.

Drain and maintain the air system, service its filters and separators, and keep hoses and connections clean. Include the point-of-use equipment in maintenance rather than focusing only on the compressor.

Spray equipment needs the same attention. Clean the gun, cup, fluid passages, and hoses with materials suitable for the coating. Residue from previous work or incomplete cleaning can enter the next application.

After cleaning, inspect the equipment before filling it. A clean container doesn't compensate for contamination farther along the fluid path.

Control mixing, storage, and handling

Keep coating containers closed between uses. Use clean mixing tools and containers, and keep their storage area separate from dirty preparation work.

Avoid returning leftover mixed material to fresh stock. Also, don't place cleaned equipment on contaminated benches or floors before assembly.

Handling the substrate can undo earlier preparation. Workers should use clean gloves where appropriate and avoid touching surfaces ready for coating.

These controls belong throughout the job, including between coats. Protecting prepared surfaces only until primer application leaves later stages exposed to the same housekeeping problems.

Trace the Source Before Continuing the Job

A useful investigation narrows the problem one variable at a time. Keep the affected area available for inspection rather than immediately sanding away every clue.

  1. Stop application and document the pattern. Photograph the defects and record when they appeared. Note whether they affect one component, a defined area, or the entire application.
  2. Review the surface history. Identify the cleaning method, preparation sequence, and handling between preparation and painting. Pay attention to areas where grease was present or difficult to remove.
  3. Examine the application path. Inspect mixing containers, tools, spray equipment, hoses, and the air supply. Look for contamination that could enter after the surface was cleaned.
  4. Compare affected and unaffected work. Review differences in substrate condition, preparation, equipment, and application timing. A defect concentrated in one area suggests a different investigation than a problem across every coated piece.
  5. Use a controlled trial before restarting. Apply the specified system to a properly prepared trial area with clean materials and equipment. Change one suspected variable at a time so the result provides useful evidence.

Record the outcome before expanding application. A successful trial supports the next decision, but it doesn't repair coating already affected.

For property owners reviewing a contractor's response, the important distinction is whether the investigation identifies a plausible source and demonstrates that the revised process avoids recurrence.

Prevention and Corrective Action Require Different Work

Prevention protects the next application

Prevention means removing contamination before painting and keeping it away during the work. It also includes using a suitable coating system and following its specified application conditions.

Film thickness and drying instructions still matter. Applying a heavier coat to hide pullback can extend drying or create a soft film. More material doesn't clean the surface underneath it.

Between coats, inspect for defects, residue, and areas needing preparation. Timing alone doesn't establish that the surface is ready.

A coating can be inside its recoat window and still need cleaning or defect repair before another coat.

Corrective action addresses the damaged film

Once fisheyes have formed, assess their extent and whether they reach the underlying coating or substrate. The repair must restore a sound, continuous film rather than cover the visible depression.

Depending on the condition, corrective work may require localized removal, cleaning, preparation, and recoating. Widespread defects can require broader removal and reapplication.

Follow the coating system's repair requirements, including preparation between layers. Our guidance on checking an industrial coating recoat window explains why elapsed time is only part of coating readiness.

Before returning to full production, address the contamination source. Otherwise, replacement coating faces the same conditions that affected the original application.

Questions to Ask Before Approving More Coating Work

Facility owners don't need to diagnose coating chemistry themselves. However, they should receive a clear explanation of what failed and what the proposed repair will address.

The contractor's response should distinguish the visible defect, the suspected source, and the work needed to restore coverage. A proposal that only adds another finish coat leaves those decisions unresolved.

Ask how the affected area will be prepared and how the next application will be evaluated. The answer should connect the repair to the observed condition. Also, document the accepted repair area so localized work doesn't leave adjacent defects untreated.

Frequently Asked Questions About Coating Fisheyes

Can another coat fill fisheyes?

Another coat may cover a depression visually, but it doesn't remove contamination beneath it. The next application can pull away again if the cause remains.

Repair decisions should address both the affected film and the condition that caused it.

Do fisheyes always expose bare material?

No. Some depressions remain within the coating, while others expose an underlying layer or substrate. Inspection needs to establish the depth and extent before repair.

Appearance alone doesn't show whether the protective film remains adequate.

Does a clean-looking surface rule out contamination?

No. Thin residue can remain on a surface that looks acceptable. Cleaning procedures, handling history, and inspection all matter.

Likewise, a smooth trial area doesn't establish that every prepared surface has the same condition.

Stop the Cause Before Recoating

Fisheyes deserve attention before another layer hides the evidence. The strongest prevention plan combines suitable surface preparation with clean equipment and protection against recontamination.

When defects appear, identify the source first and repair the affected film separately. That approach gives the next coat a sound surface instead of another opportunity to pull away.

More featured articles...

By EFC Painting • November 23, 2026
Choose an industrial painting contractor by comparing relevant experience, preparation methods, coating specifications, safety planning, and documented quality control. A strong proposal connects those elements to your facility's operating conditions and explains how crews wil...
By EFC Painting • November 22, 2026
Hotel painting in Naples fits between busy seasons when you work backward from reopening and release rooms in controlled phases. The schedule needs to protect return-to-service time , including preparation, repairs, coating application, ventilation, and inspection. A gap in re...
By EFC Painting • November 21, 2026
A solvent rub test checks how well a cured industrial coating resists a specified solvent under controlled rubbing. It can help identify a film that is still soft or vulnerable, but it does not prove that the coating is ready for every service condition. For a useful result, f...